联系人:郇海军
邮箱:shanghaiwufu@163.com
电话:18016035321
地址: 上海闵行区东川路2952号
| 型号 |
OK Autrod 309LSi |
类型 |
实心焊丝 |
| 焊接方法类型 |
气保护焊丝 |
被焊材料 |
不锈钢 |
| 加工定制 |
否 |
标准直径 |
1.2/1.6 |
| 材质 |
Austenitic (with approx. 8 % ferrite) 24 % Cr - 13 % Ni - Low C |
用途 |
适用于具有相似化学成分的锻钢和铸钢,还能够高效地用于焊接CMn钢的过渡层以及不同钢种之间的接头 |
| 牌号 |
ER309LSi |
|
供应ESAB OK Autrod 309LSi气保焊丝,欢迎洽谈采购。
ESAB OK Autrod 309LSi是一种高品质的实芯抗腐蚀铬镍合金焊丝,专为焊接含有23%铬和12%镍成分的锻钢和铸钢材料而设计。该焊丝不仅适用于具有相似化学成分的锻钢和铸钢,还能够高效地用于焊接CMn钢的过渡层以及不同钢种之间的接头。在执行过渡层和异种钢接头焊接时,严格控制焊接稀释率至关重要,以保证焊接质量的可靠性。
OK Autrod 309LSi焊丝因其的抗腐蚀性能而广受欢迎。它含有较高的硅含量,这一成分的增加显著提升了焊接过程中的浸润性及其他焊接性能。这种焊丝的杰出性能使其成为多种工业应用的理想选择,尤其在那些对高抗腐蚀性能和优异焊接性能有严格要求的场合。
ESAB OK Autrod 309LSi is a high-quality solid corrosion-resistant chromium-nickel alloy welding wire designed for welding forged and cast steels containing 23% chromium and 12% nickel. This welding wire is not only suitable for forged and cast steels with similar chemical compositions but is also highly efficient for welding transition layers of CMn steels and joints between different types of steel. When performing transition layer and dissimilar steel joint welding, it is crucial to strictly control the dilution rate of the weld to ensure the reliability of the weld quality.
The OK Autrod 309LSi welding wire is popular for its excellent corrosion resistance. It contains a higher silicon content, which significantly improves the wettability and other welding properties during the welding process. The outstanding performance of this wire makes it an ideal choice for a variety of industrial applications, especially in situations where there are strict requirements for high corrosion resistance and excellent welding performance.
| 标准:
|
EN ISO 14343-A:G 23 12 L Si, SFA/AWS A5.9:ER309LSi, Werkstoffnummer :~1.4332
|
|
认证:
|
CE EN 13479, NAKS/HAKC 1.0MM-1.2MM, CWB ER309LSi, DB 43.039.16,VdTüV 10020
|
|
合金类型:
|
Austenitic (with approx. 8 % ferrite) 24 % Cr - 13 % Ni - Low C
|
|
典型拉伸性能(AWS):
|
屈服强度:440MPa;抗拉强度:600MPa;延伸率:41%(焊态)
|
|
典型夏比V缺口冲击性能(AWS):
|
测试温度/冲击值:20℃/160J (焊态) / 测试温度/冲击值:-60℃/130J(焊态)
|
|
典型夏比V缺口冲击性能(AWS):
|
测试温度/冲击值:-110℃/90J (焊态)
|
|
典型焊缝金属成分分析%:
|
C:0.02;Mn:1.7;Si:0.9;Ni:13.5;Cr:23.4;Mo:0.15;Cu:0.12;Ferrite FN:9.0
|