| 型号 |
Techalloy 99/ERNiCr |
|
镍和镍基合金焊丝
techalloy 55 (aws无对应) techalloy 99 (aws a5.15 erni-cl) techalloy 208 fm61( awsa5.14 erni-1) techalloy 276 (awsa5.14 ernicrmo-4) techalloy 413 fm67(aws a5.7 ercuni) techalloy 418 fa60(aws a5.14ernicu-7) techalloy 606 fm82(aws a5.14 ernicr-3) techalloy 617 (aws a5.14 ernicrcomo-1) techalloy 622 (awsa5.14 ernicrmo-10) techalloy 625 (awsa5.14 ernicrmo-3) techalloy 718 (aws a5.14 ernifecr-2) techalloy 725 (aws无对应) techalloy 825 (awsa5.14 ernifecr-1)
镍和镍基合金焊条
tech-rod 55 (awsa5.15 enife-cl) tech-rod 99 (aws a5.15 eni-cl) tech-rod 112 (aws a5.11 enicrmo-3) tech-rod 117 (aws a5.11 enicrcomo-1) tech-rod 122 (aws a5.11 enicrmo-10) tech-rod 135 (aws无对应) tech-rod 141 (aws a5.11 eni-1) tech-rod 182 (aws a5.11 enicrfe-3) tech-rod 187 (aws a5.6 ecuni) tech-rod 190 (aws a5.11 enicu-7) tech-rod 276 (aws a5.11 enicrmo-4) tech-rod weld a(aws a5.11 enicrfe-2)
AWS A5.15 ERNi-CI
UNS N02215
CWB
Techalloy® 99 is used for welding of cast irons to other cast irons as well as for joining cast irons to mild steels and
stainless steels. It is also readily used for the repair of castings. The welds produced are generally more machinable than
a Tech-Rod® 55 deposit. A preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding
to prevent cracking.
DEPOSIT COMPOSITION
%C %Mn %Si %S %Fe
Requirements
AWS ERNi-CI 2.0 max. 2.5 max. 4.0 max. 0.03 max. 8.0 max.
Typical Performance
Techalloy® 99 0.003 0.07 0.09 0.001 0.1
%Ni %Cu %Al %Other
Requirements
AWS ERNi-CI 85 min. 2.5 max. 1.0 max. 1.0 max.
Typical Performance
Techalloy® 99 99 0.02 0.1